Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG13 BK00102 - PA6-GF63 - BASF

Material Data Center offers the following functions for Ultramid® B3WG13 BK00102:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Ultramid® B3WG13 BK00102 is a 63% glass filled, injection molding, high modulus Polyamid designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Applications:
Potential applications are mirror brackets, fuel lids, gas-assisted steering wheel inserts, ski bindings and bike rack clamps.
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 22400 / - MPa ISO 527
파단시 강도 235 / - MPa ISO 527
파단시 신율 2 / - % ISO 527
챠피 충격 강도 , +23°C 90 / - kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 90 / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 15 / - kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 13 / - kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 220 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 214 / * °C ISO 75-1/-2
1.5mm 평균두께에서의 난연성 HB / * class IEC 60695-11-10
테스트 두께 1.5 / * mm -
Yellow Card 유효한 예 / * - -
두께 H인 제품의 난연성 HB / * class IEC 60695-11-10
테스트 두께 3.0 / * mm -
Yellow Card 유효한 예 / * - -
기타 특성건조/응축단위시험규격
밀도 1740 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Processing humidity ≤0.03 % -
용융수지온도 300 - 320 °C -
성형온도 80 - 95 °C -
도표
점도-변형률 , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
전단-변형률 , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
응력-신율 , Ultramid® B3WG13 BK00102 (건조), PA6-GF63, BASF
응력-신율 , Ultramid® B3WG13 BK00102 (응축), PA6-GF63, BASF
시컨트탄성율-신율 , Ultramid® B3WG13 BK00102 (건조), PA6-GF63, BASF
시컨트탄성율-신율 , Ultramid® B3WG13 BK00102 (응축), PA6-GF63, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
특별 특성
열안정성
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
기타 정보
사E성
PREPROCESSING
Max. Water content: 0.03%
Although Product is supplied in sealed containers, drying is recommended in applications requiring optimum surface aesthetics. A dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

PROCESSING
Melt Temperature 300-320 °C (572-608 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500psi)
Rear Zone 275-300 °C (527-572 °F)
Center Zone 285-310 °C (545-590 °F)
Front Zone 300-325 °C (572-617 °F)
Nozzle 300-325 °C (572-617 °F)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics arecritical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.